{"data":{"id":"us/46-cfr-56.75-15","jurisdiction":"us","citation":"46 CFR 56.75-15","heading":"-15 Heating.","body":"(a) The joint must be brought to brazing temperature in as short a time as possible to minimize oxidation.\n(b) [Reserved]","path":["Title 46—Shipping","CHAPTER I—COAST GUARD, DEPARTMENT OF HOMELAND SECURITY","SUBCHAPTER F—MARINE ENGINEERING","PART 56—PIPING SYSTEMS AND APPURTENANCES","Subpart 56.75—Brazing"],"source_url":"https://www.ecfr.gov/api/versioner/v1/full/2026-08-25/title-46.xml","current_through":"2026-08-25","vintage":"","retrieved_at":"2026-08-27T02:26:22Z","sha256":"00653db0b64b48c003a4338e9e598ba21bffaa046adc9ea2cf582a292fca460a","source_id":"us-cfr","stale":true,"prev":"us/46-cfr-56.75-10","next":"us/46-cfr-56.75-20"},"notice":"GroundRules: Original legal text. Not legal advice."}