49 CFR 192.489: Remedial measures: Cast iron and ductile iron pipelines.
Where this section sits in the code
- Title 49—Transportation
- Subtitle B—Other Regulations Relating to Transportation
- CHAPTER I—PIPELINE AND HAZARDOUS MATERIALS SAFETY ADMINISTRATION, DEPARTMENT OF TRANSPORTATION
- SUBCHAPTER D—PIPELINE SAFETY
- PART 192—TRANSPORTATION OF NATURAL AND OTHER GAS BY PIPELINE: MINIMUM FEDERAL SAFETY STANDARDS
- Subpart I—Requirements for Corrosion Control
(a) General graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced.
(b) Localized graphitization. Each segment of cast iron or ductile iron pipe on which localized graphitization is found to a degree where any leakage might result, must be replaced or repaired, or sealed by internal sealing methods adequate to prevent or arrest any leakage.